← 返回案例库
水处理/环境相关FeNiAngewandte Chemie International Edition

Corrosion‐Driven Ni3S4 Gradient in NiFe‐LDH Enables Durable Industrial‐Scale Water Electrolysis

Corrosion‐Driven Ni3S4 Gradient in NiFe‐LDH Enables Durable Industrial‐Scale Water Electrolysis

研究概述

研究内容请参见论文原文。

谱图与表征信息

图2 · 原文PDF第5页
Figure 2. Electronic structure analysis of NiFe-LDH and Ni3S4/NiFe-LDH. a) XPS image of NiFe-LDH by Ar+ etching of different profiles of Fe 2p. b) Ni K-edge XANES spectra of Ni foil, NiO, NiFe-LDH, and Ni3S4/NiFe-LDH. c) Fe K-edge XANES spectra of Fe foil, Fe2O3, NiFe-LDH, and Ni3S4/NiFe-LDH. d) XPS image of Ni3S4/NiFe-LDH by Ar+ etching of different profiles of Fe 2p. e) Ni K-edge k3-weighted FT-EXAFS spectra at R space. f) Fe K-edge k3-weighted FT-EXAFS spectra at R space. g) XPS image of NiFe-LDH by Ar+ etching of different profiles of Fe 2p. Wavelet transform of k3-weighted EXAFS data for Ni K-edge of h) NiFe-LDH and i) Ni3S4/NiFe-LDH. j) XPS image of Ni3S4/NiFe-LDH by Ar+ etching of different profiles of Ni 2p. Wavelet transform of k3-weighted EXAFS data for Fe K-edge of k) NiFe-LDH and l) Ni3S4/NiFe-LDH.
咨询选型申请测试
图片放大