← 返回案例库
FeJournal of Hazardous Materials

Temperature-induced atomic intrinsic sites evolution during waste dyeing sludge into the wealthy iron-based catalyst to sustainable decontamination

Temperature-induced atomic intrinsic sites evolution during waste dyeing sludge into the wealthy iron-based catalyst to sustainable decontamination

研究概述

研究内容请参见论文原文。

谱图与表征信息

图3 · 原文PDF第5页
Fig. 3. (a) Normalized Fe K-edge XANES spectra of as-prepared catalysts and reference samples (i.e., Fe foil, FeO, Fe2O3, and Fe3O4) and (b) the corresponding Fe composition ratio based on LCF-XANES fitting. (c) k3-weighted Fourier transformed EXAFS spectra of the as-prepared catalysts and reference samples (i.e., Fe foil, FeS, and Fe2O3). (d) Schematic diagram of the structural changes with temperature-dependent.
图6 · 原文PDF第9页
Fig. 6. (a) Fe compositions based on LCF-XANES fitting and (b) C, N, Fe, and S composition ratios based on XPS fitting of used BC-800. (c) Variation in Fe2+, total iron, and PMS concentrations in the solution. (d) Photographic image of the continuous flow device. (e) 4-CP removal efficiency over 24 h using the membrane system experimental setup.
咨询选型申请测试
图片放大