← 返回案例库
锂电池相关NiJournal of Energy Chemistry

Mitigating kinetic hindrance of single-crystal Ni-rich cathodes through morphology modulation, nickel reduction, and lithium vacancy generation achieved by terbium doping

Mitigating kinetic hindrance of single-crystal Ni-rich cathodes through morphology modulation, nickel reduction, and lithium vacancy generation achieved by terbium doping

研究概述

研究内容请参见论文原文。

谱图与表征信息

图2 · 原文PDF第4页
Fig. 2. (a) Ex-situ XANES spectra of the pristine SNCM and SNCM-Tb1 at the Ni K-edge with insets showing the pre-edges and zoomed-in peaks. (b) Fourier transformation of EXAFS. 2D Fourier transformed Ni K-edge EXAFS spectra for (c) SNCM and (d) SNCM-Tb1 materials.
咨询选型申请测试
图片放大