RESEARCH / A0109

Interfacial anchoring of manganese boosting cycle stability of__LiMn0.6Fe0.4PO4 cathode for lithium-ion battery

Lithium batteriesMnElectrochemistry Communications

Read the original paper · 10.1016/j.elecom.2026.108189 ↗

Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.

Figure 1 · PDF page 2
Fig. 1. (a) XRD patterns for LMFP@C and LMFP@C/S; (b) S 2p spectrum of LMFP@C and LMFP@C/S; (c) HR-TEM images of LMFP@C/S (Appendix: EDS Mapping image of S, Mn, Fe, P and O elements); (d) Mn K-edge XANES spectra; (e) Mn K-edge EXANES spectra.
Discuss a systemSample evaluation
Enlarged source figure