Enhanced coking and sintering resistant in dry reforming of methane over CoRh alloy confined in mesoporous silica

CoRhApplied Catalysis B: Environment and Energy

Read the original paper · 10.1016/j.apcatb.2026.126584 ↗

Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.

Figure 2 · PDF page 5
Fig. 2. (a) H2-TPR profiles on various catalysts. (b) CO-DRIFTS spectra. (c) Co K-edge XANES profiles. (d) Co EXAFS spectra. (e) Rh K-edge XANES profiles. (f) Rh EXAFS spectra. Wavelet transform (WT) spectra of the Co K-edge for (g) Co foil, (h) Co3O4, (i) Co7Rh3/DMS (reduced state), (j) Co7Rh3/DMS-OX (oxidized state).
Discuss a systemSample evaluation