ZnN Interface Bridges for Dual-Function Enhanced Photocatalytic H2O2 Production
Read the original paper · 10.1016/j.apcatb.2026.126419 ↗
Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.
Fig. 1. SEM image of ZnO (a) and ZP10 (b); EDS mapping of ZP10 (c); HRTEM image (d) and Color-enhanced HRTEM images (e) of ZnO; XANES (f) and FT-EXAFS (g) spectra of Zn foil, ZnO, ZnPc, and ZP10. FT-EXAFS fitting curves of ZP10 (h); Wavelet transform k2-weighted EXAFS spectra of Zn foil, ZnO, ZnPc, and ZP10 (i-l).