RESEARCH / A0241

Surface exposure engineering of highly active Mn-based spinel in monolithic catalysts for efficient acetone degradation

MnJournal of Hazardous Materials

Read the original paper · 10.1016/j.jhazmat.2025.139780 ↗

Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.

Figure 3 · PDF page 4
Fig. 3. (a) Pore size distributions; (b) Mn 2p XPS spectra; (c) The normalized X-ray absorption near-edge spectra at the Mn K-edge; (d) O 1 s XPS spectra; (e) EPR spectra; (f) O2-TPD.
Discuss a systemSample evaluation
Enlarged source figure