RESEARCH / A0296

Interface-engineered ZnO/FeCu-SSZ-13 with robust SO2 and H2O resistance for low-temperature NH3-SCR

ZnChemical Engineering Journal

Read the original paper · 10.1016/j.cej.2025.167119 ↗

Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.

Figure 5 · PDF page 26
Fig. 5. (a) Zn K-edge in situ XAFS spectra under different atmospheres, and (b) SO2+O2-in situ
Discuss a systemSample evaluation
Enlarged source figure