Tailored binder to eliminate the concentration polarization in ultrathick electrodes for lithium battery

Lithium batteriesCuJournal of Power Sources

Read the original paper · 10.1016/j.jpowsour.2025.237375 ↗

Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.

Figure 3 · PDF page 4
Fig. 3. (a) Cu LM2 XPS spectra of the reaction products between SPAN and CuSO4. (b) Cu K-edge EXANES and (c) FT-EXAFS spectra of the reaction products of SPAN with CuSO4. (d) Electronic conductivity of the SPAN electrodes. (e) SEM picture of the surface morphology of βPC electrode with Cu EDS spectra inserted. (f) Crosssection SEM and EDS images of the βPC electrodes.