RESEARCH / A0535

Enhanced Photocatalytic Nitrogen Fixation over Nano-UiO-66(Zr) via Natural Chlorophyll Sensitization

Photocatalysis / photoelectrocatalysisZrInorganic Chemistry

Read the original paper · 10.1021/acs.inorgchem.4c04391 ↗

Source figures may contain other techniques and soft X-ray spectra. C, N and O measurements are outside our current hard-XAFS testing range.

Figure 3 · PDF page 4
Figure 3. Plot (αhν)2 versus hν of (a) UiO-66 and (b) Chlor@UiO-66. (c) Photoluminescence (PL) spectroscopy. The high-resolution XPS spectra of (d) Zr 3d, (e) C 1s, and (f) N 1s. (g) Normalized Zr k-edge XANES spectra with a Zr foil as the reference (the inset shows the near-edge portion). (h) R space and (i) wavelet transforms for Zr k-edge EXAFS of UiO-66 (upper) and FC@UiO-66e (down).
Discuss a systemSample evaluation
Enlarged source figure